Rauvolfia vormitoria Effect on the Degradation of Aluminium Alloy in 2.5 M Hydrochloric Acid Solution
The deterioration of aluminium alloy in 2.5 M hydrochloric acid in the presence Rauvolfia vormitoria extract was examined using both gasometric and gravimetric techniques. Aluminium coupons measuring 4 cm by 1 cm were introduced into test solutions of uninhibited acid and also those containing extract quantities of 10, 20, 30 and 40 cm3 at ambient temperature of 250C for a total cumulative...
Ajayi, O.O., Joseph, O.O., Omotosho, O.A. and Olabowale, T.O